316/316L is the most commonly used austenitic stainless steel in the chemical process industry. The addition of molybdenum increases general corrosion resistance, improves chloride pitting resistance and strengthens the alloy in high temperature service. Through the controlled addition of nitrogen it is common for 316/316L to meet the mechanical properties of 316 straight grade, while maintaining a low carbon content.
In what form is Stainless Steel 316 available at ISHWAR STEEL CORPORATION?
Ni | Cr | C | Mo | Mn | Si | C | S | P | N | Fe | |
---|---|---|---|---|---|---|---|---|---|---|---|
MIN | 10.0 | 16.0 | 2.0 | - | - | - | - | - | - | - | - |
MAX | 14.0 | 18.0 | 3.0 | 2.0 | 0.75 | 0.03 | 0.03 | 0.03 | 0.045 | 0.1 | Balance |
AMS 5507
AMS 5648
ASM5653, ASTM SA 240
ASTME SA312
ASME SA-479
ASTM-240
ASTM A 276
ASTM A 276 Condition,ASTM A 276 Condition A
ASTM A 276 Condition S
ASTM A 312
ASTM A 479
EN14404 UNS S31600, UNS S31603
W. Nr./EN 1.4401
Werkstoff 1.4404
316 / 316L Bar, 316 / 316L Coil, 316 / 316L Concentric Reducers, 316 / 316L Flanges, 316 / 316L Hex Bar, 316 / 316L Pipe, 316 / 316L Plate, 316 / 316L Round Bar, 316 / 316L Sheet, 316 / 316L Stub Ends, 316 / 316L Tees, 316 / 316L Welding Products
316 Stainless, 316L Stainless
Temperature, °F |
70 | 212 | 932 | 1832 |
Coefficient* of Thermal Expansion, in/in°F x 10-6 |
- | 9.2 | 10.1 | 10.8 |
Thermal Conductivity Btu • ft/ft2 • hr • °F |
7.8 | - | - | - |
Modulus of Elasticity Dynamic,psi*106 • |
29 | - | - | - |
Representative Tensile Properties
Minimum | Typical | |
Ultimate Tensile Strength, ksi |
75 | 90 |
0.2% Yield Strength, ksi |
30 | 35 |
Elongation, % |
40 | 60 |
Temperature, °F | 70 | 200 | 400 | 600 | 800 | 1000 | 1200 | 1400 |
Ultimate Tensile Strength, ksi | 82.4 | 75.6 | 71.1 | 71.1 | 71.1 | 68.4 | 50.7 | 30.7 |
0.2%Yield Strength, ksi | 42.4 | - | - | - | 26.5 | 23.4 | 22.6 | - |
Charpy Impact V-notch,ft-lbs | 65-100 | - | - | - | - | - | - | - |